    I've been enjoying using my Avus 9 x 12 a lot lately. Shooting sheet film and roll film in a Suydam back. I just got 24 plates to try in it. They are long expired but very slow speed so I'm hoping not too fogged. Anyway. Do I need a developer that is hardening for glass plates? Any recommendations? I have some Original Microdol mixed up that works great that I might try. It's from the 1950s before they changed the formula. It works great with Fomapan btw.
    Another thing, I scored some Zeiss film holders that were miss marked on the big auction site. One is unused in the original packaging which has a big caution printed on the front to be sure to store them without the dark slide in them so as not too compress the light trap. The first time I'd seen that. Too bad they didn't caution people to store them with moth balls eh?
    greg
     
  2. ntenny

    ntenny Member

    Messages:
    2,284
    Joined:
    Mar 5, 2008
    Location:
    San Diego, C
    Shooter:
    Multi Format
    I've always used HC-110 for old plates, for its fog control. I don't think Microdol contains any antifoggants, does it?

    I suppose historically a hardener would have been used, but I haven't, and things *seem* to be OK, although I don't go around beating up plate emulsions to see if they needed more hardening.

    -NT
     
  3. GregW

    GregW Member

    Messages:
    185
    Joined:
    Dec 10, 2012
    Location:
    East Coast
    Shooter:
    Multi Format
    Thanks Nathan. yes, I think you're right, I think The "X" was an antifoggant? I have some Benzotriazole stuff I could dose the microdol with. I just opened one of the packages and it had some recipes inside for developing etc. It said if you would like to harden the plates use a fixer with hardener. So I won't worry. The first developer is a Pyro developer the second is a Metol etc type. It gives a 4 minute development time btw ?! This is Panchromatic so I can't develop it and observe. I'm going to try 10 minutes in the microdol. I exposed the test plate at asa 12. I'll order some HC-110 for the future.
     
  4. paul ron

    paul ron Member

    Messages:
    1,443
    Joined:
    Jan 22, 2004
    Location:
    NYC
    Shooter:
    Medium Format
    I'm enjoying reading all these great post on plate.

    I have a Maximarr 9x12 l have been wanting to shoot but lack on info n materials has kept in the dark so many years.

    Please let me see how it turns out for you?

    Thanks
     
  5. Simon Howers

    Simon Howers Subscriber

    Messages:
    99
    Joined:
    May 21, 2011
    Location:
    West Yorkshi
    Shooter:
    Large Format
    Maco do a hardening solution which can be added to developer. It's marketed as part of their emulsion package but can be bought separately. It is recommended by Christopher James in his book Alternative Photographic Processes (2nd edition) for use with dryplates.
     
  6. Ole

    Ole Moderator Staff Member

    Messages:
    9,284
    Joined:
    Sep 9, 2002
    Location:
    Bergen, Norw
    Shooter:
    Large Format
    Any staining developer is hardening. Pyrocat, for example.
     
  7. jnanian

    jnanian Advertiser

    Messages:
    19,121
    Joined:
    Jun 21, 2003
    Location:
    local
    Shooter:
    Multi Format
    hi

    mark osterman suggested on his dry plate page
    ( i have to find it, i can't remember where it is ! )
    to use a very active developer and develop the plate for a long time ...

    the plates i get the best images from seem like they are over processed
    ( compared to film or paper ) but they print on a hard paper like azo or lodima &c
    nicely :smile:

    hardener is a swell idea (sorry for the bad pun ) ..