Morten,
a common method is "double clearing time for conventional films, tripple clearing time for t-grain stuff".
Estimate the clearing time with a piece of undeveloped film (like the film leader tongue) and watch it clear completely, then use that base time. Once the clearing time doubles in relation to the base time, the fixer is spent and should be replaced with fresh fix (or bath two fix).
__________________
Tschüss,