View Single Post
Old 11-13-2006, 07:54 PM   #1 (permalink)
mikebarger
 
Join Date: Jan 2005
Location: south central Missouri
Posts: 789
Default Hypercat Staining Developer

Mix the chemicals in order, all should dissolve between 120 and 150 degrees.

You should try 1:6:200 at 70 degrees for printing on VC paper with HP5 4x5 film.

A fellow on Photo.net stated he is using 1:1:300 for semi-stand FP4 35mm.

Like any of the two solution developers it looks like there is a range of possibilities for ratios and development methods.

While I'll probably stick with the 510 Pyro, I like the one solution rather than two, have any of you tried the Hypercat? I'd like to hear your results.

Mike