I think I may have a cure to the problem.
First I added 30% more gelatin to the ready made batch of emulsion.
Next I set the exposed plate in a .5gm Alum : oz. water solution for one minute, developed in usual dektol 1:1 with cyanate.
Other option was to use developer D-19 undiluted with cyanate, no hardening required but the development time shuld be increased by 50%. |