I use it with ABC in 8x10 and 5x7 sheets. I brush develop by inspection individual negatives for bout 4 minutes at 75F. Give or take a minute or two for expansion and contraction as needed. I've also use the film with Pyrocat HD in 120 and 135. I semi-stand develop those at a 1:1:150 dilution for anywhere from 30min to 1 hr depending on the temperature. You can expect to get full speed out of the stand developed PCat...sometimes more...