Yep and I'm not the only one who's complaining. Its been an issue labs here have had for years but like most product complaints in Australia.... Theres never any change. I'de love to know is this is a world wide product issue or weather its just Australia gets short changed.
no. its simply a case of buy it knowing your not getting the full lenghts worth and consider it lucky we have the materials at all. I should mention that the problem is worse with kodaks papers than fuji's. Do you think I should complain to Kodak USA about this issue?
"Its my profession to hijack time" ~ Stephen Frizza.
Hi Stephen. Could you describe the surface defect? I use quite a bit of roll paper here in the northeast U.S. and I've never witnessed any surface issues in either F or N. Are you in a particularly humid area? Are you in the habit of refrigerating your stock?
no. its simply a case of buy it knowing your not getting the full lenghts worth and consider it lucky we have the materials at all. I should mention that the problem is worse with kodaks papers than fuji's. Do you think I should complain to Kodak USA about this issue?
Steve;
Complain to Kodak USA, by all means.
This could be a shipping problem related to long rolls and the center parts getting more abrasion. Abrasion is adjusted by ingredients in the top coat. If the top coat is left off, the top layer can be completely fogged due to abrasion.
So, I suspect that they can do something about it.