    Processing 4 rolls of 120s with CPE2

    Hi,

    I've been processing two 120s on a 2502 reel with a 2521 multi-tank (CPE-2) and would like to process at least 4 rolls of 120s at the same time but jobo thing is a bit confusing...

    1. Do I need a 1520 tank with two 1501 reels? or is it a 1540 tank with two 1501 reels?
    2. I've heard that I might have an unevenness problem since the 1501 reel is smaller than 2502. Is it true?
    3. How much ml developer and blix do I need for 4 120s? Double it to 600 ml? or more?

    Many thanks in advance!
    Last edited by rustyair; 07-21-2013 at 11:21 PM. Click to view previous post history.

  2. #2
    polyglot's Avatar
    Join Date
    Jun 2009
    Location
    South Australia
    Shooter
    Medium Format
    Posts
    3,233
    Images
    12
    2xxx reels require 2xxx tanks, etc; the 1xxx tanks are smaller diameter.

    This is the link you need.

    I use a Multitank 5 (2551) with 3 of 2502 to develop 6 rolls at a time; needs about 700mL.

  3. #3

    Join Date
    May 2011
    Location
    MA, USA
    Shooter
    Large Format
    Posts
    1,243
    Images
    19
    You want the 1540 with 2X 1501 reels if you want to use less chemistry.
    You only need 470ml when running 4 rolls in the 1540.

    You will not see any difference between 1501 an 2502 reels in processing.
    CatLABS of JP
    Darkroom resources and service

    www.catlabs.info | https://www.facebook.com/CatLABS.of.JP | www.jobo-usa.com



 

APUG PARTNERS EQUALLY FUNDING OUR COMMUNITY:



Contact Us  |  Support Us!  |  Advertise  |  Site Terms  |  Archive  —   Search  |  Mobile Device Access  |  RSS  |  Facebook  |  Linkedin