Quote Originally Posted by Photo Engineer View Post
Great work. Congratulations.

At that concentration of NaBr after the wash, at 10 deg C (a good wash temp), the vAg would be about +37 and at 40 deg C (a good coating temp) it would be about +67 mv.
PE
Can you show the math behind these calculations?

Thanks,

Ray