I shoot a lot of Efke 100 in sizes from 120 roll through 8x10 sheet. I develop most of it in Pyrocat-HD with no stop bath (plain water instead) and an alkaline non-hardening fixer.

Absolutely no pinholes! No problems with emulsion softness (that I didn't create)!