Increasing the temperature will increase the activity of the developer. It will also soften the emulsion a bit more. Both these factors will contribute to slightly coarser grain.

Pushing HP5 in Ilfosol S will also give coarse grain...

Most of my MF negatives are FP4, developed in Ilfosol S at 24C. A beautiful combination...