I apologize that my original explanation was less than complete.

My Process is:
1 minute developing in Liquidol paper developer.
30 second total stop bath, plain water - two bath
30 second fixer, TF-3
Brief wash
4 minute selenium toner 1:9 dilution
3 minute wash
hang to dry

The problem is that when I try to remove the dry prints from the line, the paper de-laminates. and you can see the paper under the plastic coating. This has happened with both Ilford and Adox papers. Neither paper manufacturer makes the paper so I question if there has been a change with the substrate. I have never had this happen in the past, even with test strips that were left in water for hours. Ilford recommends keeping the wetted time under 15 minutes and I am careful to do that.