I successfully processed Tri-X exposed at 160ASA in Foma LQR, which is the developer included in the Foma Reversal Kit. I used it diluted 1+6 at around 12 min, 20C, with no problems. See yourself : https://vimeo.com/39136131

For advice, I would suggest you to try plain Rodinal as 1st and 2nd developer, diluted 1:15 (66mL/L), 1st developing for around 10 min at 20C. Browse my other vids for more details...