Hi, I am processing my own slide film (Provia 100F) in my Jobo processor. I am processing 35mm, 120, and 4x5 sheets. The most troublesome from a curling standpoint is the 35mm, but I am getting curl in my 120 and oddly enough a little bit in my 4x5 sheets. The 120 roll film and 4x5 is manageable, but the 35mm is really an issue. When I used to send the 35mm and 120 out to my local lab, it always came back very flat.

Any ideas when self-processing, how to address this curling issue with the E-6 roll film? I only shoot Provia 100F, so I am not sure if this has anything to do with it, but wanted to mention that just in case. I am using the Arista 3 Bath Kit which is processed at 105F/45C which is 5 degrees warmer than the traditional E-6 kits, so I am wondering if this has anything to do with it.