Gold only Sal. I believe I did 1 min or so of a MGIV and WT in 105 degrees of T-26.

Is cold sharp steely crisp....I love cold tone so much I now only use Slavich Unibrom (a bromide paper). Same deal 1 min or so in T-26 at 105F and you're good t'a go. Selenium after gold makes it all funky. Some like it but selenium always warms or purples it too much for me. Gold toned paper (T-26) is archival fwiw, selenium isn't required, unless you want those neat colors (they aren't my cuppa tea...but hey we can't all be the same )