Not sure why the emulsion is seperating. I use this combination often and have never had this problem. I aslo use TF-4 for the same amount of time. The magenta stain seems to be normal, as I have got it every time. Not to mention the film curls like a mad dog. Perhaps you just got a bad batch of film. Try another developer and see if you get the same results to be sure.