Quote Originally Posted by John_Brewer
Sandy, it could well be the same film, the label sealing the film bag has Chinese writing on it. I would be very interested in seeing your data.

Gerhard, thanks for your info.


If it is the same film I would recommend about eight minutes of development at 72F, using the 2:2:100 dilution of Pyrocat-HD. This should give you a DR of about 1.75, which would be about right for palladium with a bit of Na2.

This is based on rotary processing and is for scenes of normal contrast.