Many people have wondere about dry ferrotypes other than Rockland kits, the only secret ingredient is the addition of .5 gm Ammoniumthiocyonate to each ounce of Dektol developer at a 1:1 working strength, develop 2 min.

Exposure test for me was F:32, 8 sec, sunny day.