Quote Originally Posted by sanking
Jim,

10 minutes at 75 degrees F with the 1:1:100 dilution of Tmax 400 film should have given you plenty of contrast for silver printing. The high reading of log 0.65 suggests to me that the developer is either bad or was not mixed correctly.

Sandy King
Thanks Sandy.

I purchased the Pyrocat-HD kit from Bostick & Sullivan so I assume that the chemicals are O.K.

I guess I could have mixed it wrong. Wouldn't be the first time I screwed something up 1oz Part A / 1oz Part B / 100oz Water?

I'll try another batch tonight when I get home from work and see how they turn out.

Thanks again!

Jim