For film, glyoxal or chrome alum or both in a mixture, but for plates only chrome alum is suggested.

Be careful of chrome alum with some sensitizing dyes. It will harden faster with some dyes due to an interaction of some sort. I have had one small batch with chrome alum set up on me during the coating session.

PE