Hi Bill - I use glyoxal now as a substitute for formalin in my hardner. I use the same concentration, and it works well. This is the hardner I use on the matrix after it has been washed off. This makes for a much more durable matrix. Not sure how it would work in an emulsion though, that is a much more complex thing.

Regards - Jim